Remote Controlled Systems for Theranostics

Name
Gleb
Surname
Sukhorukov
Scientific organization
Queen Mary University of London
Academic degree
Professor
Position
Professor
Scientific discipline
Chemistry & Chemical technologies
Topic
Remote Controlled Systems for Theranostics
Abstract
The talk will review recent advanced in development of remote controllable delivery systems, where micro- and nanostructured carriers can be addressed via light, magnetic field and ultrasound resulting on their navigation and deploy of cargo at designated area
Keywords
Delivery systems, polymers, nanoparticles, encapsulation