Experimental studies of non-uniform fields of displacements and deformations during the quasi-static and dynamic tensile testing, punching, spinning the reinforcing fibers
Abstract
The results of studies of the properties of the reinforcing fibers; an analysis of the mechanisms of deformation and destruction of samples of woven materials during the quasi-static and dynamic tensile testing, punching, drawing fibers using non-contact digital optical strain field analysis system.
Keywords
quasi-static testing, dynamic testing, tensile testing, punching, spinning, reinforcing fibers, DIC