Регистрация / Вход
Прислать материал

nanomedicine & drug delivery, pharmacoengineering

Name
Alexander
Surname
Kabanov
Scientific organization
University of North Carolina at Chapel Hill (primary) M.V. Lomonosov Moscow State University (secondary)
Academic degree
Dr. Sc. (доктор химических наук)
Position
Professor and Director Center for Nanotechnology in Drug Delivery
Scientific discipline
Chemistry & Chemical technologies
Topic
nanomedicine & drug delivery, pharmacoengineering
Abstract
“Nanozyme” technology incorporates proteins into nanosized core-shell polyion complex particles that preserve even very fragile proteins in biological milieu, decrease their clearance and allow their site-specific delivery across cellular barriers. Examples include nanozymes based on antioxidant enzymes , scavengers of organophosphorous toxins and neurotrophins for treatments of obesity, stroke, Parkinson’s disease, RETT syndrome, organophosphorous toxins poisoning, and some others.
Keywords
nanomedicine, nanozyme, drug delivery