Abstract
Market research showed that despite the high cost of bulk nanostructured materials produced by the SPD techniques, their application in medicine is of great interest. This is due to high biomechanical properties of nanomaterials and, hence the possibility to fabricate high-strength designs with reduced weight and size parameters. The development of innovative ideas in the field of nanomaterials’ application in medicine offers the challenge of performing scientific and applied work in order to develop wires, plates and other semi-products of nanostructured metals.
Keywords
nanomaterials, medical implants
Summary

no