New materials, Manufacturing technologies & Processes
Topic
Innovative materials based on thermoplastic polymers
Abstract
Modern composite materials based on thermoplastic polymers possess unique set of properties and could be used as a replacement for traditional construction materials in automotive, aerospace and shipbuilding industry. Development of such material requires deep understanding of relationship between their structure and properties. Multiscale computer simulation accompanied by experimental studies is one of the most advanced methods to study such materials, and predict their properties.
Keywords
multiscale computer simulation, composite materials, molecular dynamics, thermoplastic polymers