Optics of spin noise in semiconductors
Name
Valerii
Surname
Zapasskii
Scientific organization
Spin Optics Laboratory, St.-Petersburg State University
Academic degree
Doctor of Sciences
Position
Leading Researcher
Scientific discipline
Physics & Astronomy
Topic
Optics of spin noise in semiconductors
Abstract
The spin noise spectroscopy represents, at present, a new, highly efficient method of research with unique and somewhat curious properties. Generally, it does not imply any perturbation of the system and, at the same time, may exhibit properties more typical for nonlinear optics. During the last several years, many new opportunities provided by the spin-noise technique have been discovered and used for studying spin-system dynamics in semiconductors. Recent results show that the spectroscopy of spin noise is a promising method of research with still underestimated potential.
Keywords
spin noise spectroscopy, spin dynamics, magnetic resonance, magneto-optics